#7 |
Senior Member
Join Date: Oct 2002
Location: Pittsburgh
Posts: 575
Likes: 298
Liked 747 Times in 136 Posts
|
![]()
Aluminum is a terrible material for fatigue resistance. Horrible.
A quality steel rod (not made in China) will last essentially a lifetime if kept within its design range. Not so with aluminum no matter what the alloy, or QA/QC. Its just the nature of the materials inherent poor fatigue resistance qualities. Oliver and Manley offer very reasonably priced 100% USA material, USA forging, and USA machined rods... right around $1200 a set. |
![]() |
![]() |
|
|