Anodized Ring Lands
Anybody have any experience or used such? My top ring to land ware pattern is lacking making 360* contact. 2nd ring without anodizing on land has nice ware pattern as if it was a top ring. It looks like the top ring is allowing a lot of cylinder pressure to get to the second ring. Both are steel rings. I will lap top ring on surface plate to check for flatness.
|