Cool Re: Hard Blok - Block Filler

Make sure all freeze plugs are out, hot tank, wash out and then use only brass freeze plugs before using muriatic acid.Make sure the drain plugs are out, rinse and dry the block thouroughly, then install the filler one side at a time as was suggested with a day or two in between. Take your time and do it right, as I know of no way to get this stuff out if you do it wrong.Make sure you do the acid in a well ventilated place because it will stink up the place, and the fumes are corrosive.